| 性能項目 | 試驗條件[狀態] | 測試方法 | 測試數據 | 數據單位 | |
| 基本性能 | 熔體流動速率 | ASTM D-1238 | 4.5 | g/10min | |
| 乙烯基醋酸鹽含量 | HCC Method | 26 | % | ||
| 密度 | ASTM D-1505 | 0.949 | g/cm3 | ||
| 機械性能 | 抗張強度(破斷點) | ASTM D-638 | 170 | kg/cm2 | |
| 破斷點伸長率 | ASTM D-638 | 800 | % | ||
| 硬度 | ASTM D-2240 | 82 | Shore A | ||
| 硬度 | ASTM D-2240 | 28 | Shore D | ||
| 熱性能 | 維卡軟化點 | ASTM D-1525 | 48 | ℃ | |
| 熔融點 | ASTM D-3417 | 76 | ℃ | ||
| 低溫脆化溫度 | ASTM D-746 | <-76 | ℃ | ||